氧化鋁空心球磚主要是以氧化鋁空心球為主要原料,以剛玉細粉做添加物,在高溫1800度窯爐內燒制而成。它具有抗高溫,熱穩定性好,保溫效果優良等特點。近年來廣泛用于高溫推板電窯、遂道窯、梭式窯爐等各種高溫工業窯爐高溫區域。使用效果持久耐用,為企業創造了經濟效益。
項目Ltem |
氧化鋁空心球磚 Alumina bubble brick |
氧化鋯空心球磚Zirconia bubble brick |
||||
|
85磚 |
87磚 |
90磚 |
95磚 |
99磚 |
98磚 |
AL2O3% |
≥85 |
≥87 |
≥90 |
≥95 |
≥99 |
- |
ZrO2% |
- |
- |
- |
- |
- |
≥98(含穩定劑) |
SiO2% |
≤13 |
≤12 |
≤8 |
≤4 |
≤0.2 |
≤0.2 |
Fe2O3% |
≤0.3 |
≤0.2 |
≤0.2 |
≤0.2 |
≤0.2 |
≤0.2 |
體積密度g/cm3 Bulk density |
1.2-1.7 |
1.3-1.5 |
1.4-1.7 |
1.4-1.7 |
1.4-1.7 |
2.5-3.5 |
常溫耐壓強度MPa Cold crushing strength |
≥12 |
≥10 |
≥10 |
≥10 |
≥9 |
≥8 |
荷重軟化開始溫度℃(0.1MPa ,0.6%) Refractoriness under load |
≥1650 |
≥1650 |
≥1700 |
≥1700 |
≥1700 |
≥1700 |
重燒線變化率%(1600℃x3h) Reheating linear change |
±0.3 |
±0.3 |
±0.3 |
±0.3 |
±0.3 |
±0.2 |
熱膨脹系數x10-6(室溫-1300℃) Thermal expansion coefficient |
~7.8 |
~7.8 |
~8.0 |
~8.0 |
~8.6 |
~9.1 |
導熱系數 w/(m.k)(平均溫度800℃) Thermal Conductivity
|
≤0.8 |
≤0.8 |
≤1.3 |
≤1.4 |
≤1.5 |
≤0.3 |
最高使用溫度℃ Max service temperature |
1680 |
1700 |
1700 |
1700 |
1800 |
2200 |